ʻO nā ʻāpana Polyamide 6—i ʻike nui ʻia ʻo Nylon 6 chips—ua kapa ʻia no nā loulou amide (–CO–NH–) i loaʻa i loko o kā lākou macromolecules. ʻIke pinepine ʻia he mau granules cylindrical keʻokeʻo, ʻo nā ʻāpana Nylon 6 he 210–220°C ka melting point a me ka mahana decomposition ma kahi o 300°C. Hiki ke hoʻoheheʻe ʻia i loko o ka phenol a me ka sulfuric acid i hoʻohuihui ʻia, hōʻike i nā waiwai insulation uila maikaʻi loa, a loaʻa iā lākou ke kūpaʻa maikaʻi i ka alkalis a me ka corrosion. ʻO Nylon ka mea kūpaʻa loa i ka abrasion o nā olonā synthetic āpau.
ʻO ka milo lole no nā lole, ka olonā ʻoihana a me ka olonā, nā ʻiliʻili Co-Extrusion.
Ka hoʻopili ʻana
ʻEke Jumbo 800Kg, 28MT/40HQ
Waiwai
ʻAno Hoʻāʻo
Nā Kūlana Hoʻāʻo
ʻĀpana
Hopena Hoʻāʻo
Papa
LX340
Ka mānoanoa pili
/
25℃, 96%H2SO4, m:v = 1:100
/
3.40±0.03
Ikaika hoʻopaʻa
ASTM D638
50mm/min
Mpa
72.37
Ka hoʻoluhi ʻana i ka wā haki
ASTM D638
50mm/min
%
82.59
Ikaika kūlou
ASTM D790
2mm/min
Mpa
94.89
Modulus Flexural
ASTM D790
2mm/min
Mpa
2187.19
Ikaika hopena
ASTM D256
23℃
kJ/m²
2.68
Ka nui o ke kahe ʻana o ka nuipa heheʻe
ASTM D1238
235℃, 2.16kg
g/10min
5.90
Hoʻokuʻu ʻōlelo:
ʻO nā helu ma luna nei he mau waiwai maʻamau no ka moʻo huahana like, i lawelawe ʻia ma ke ʻano he kuhikuhi no ke koho ʻana o ka mea kūʻai aku i nā huahana, a ua kau ʻia nā waiwai maoli i ka COA o ka huahana.